Structural Behaviour of Eco-Coastal Alkali-Activated Slag-Based Wave-Impact-Resistant Blocks Containing Recycled Seashell Aggregates under Marine Exposure

Noor Muhammad Rafai

NED University of Engineering and Technology (NEDUET), Karachi, Pakistan

Sadullah Younas Gondal

ECEC - East Consulting Engineering Company, Jeddah, Kingdom of Saudi Arabia

Fammaz Ali

Structural Engineer, Coventry University, United Kingdom (UK)

Muhammad Munawar

Tehsil Officer (I&S), Local Government Department, Khyber Pakhtunkhwa, Pakistan

Maaz khan

University of Engineering and Technology (UET), Peshawar, Pakistan

Saiful Islam

University of Engineering and Technology (UET), Peshawar, Pakistan

Muhammad Mudassar Abbas

University of Engineering and Technology (UET), Taxila, Pakistan

Keywords: alkali-activated slag, recycled seashell aggregate, coastal protection, wave impact, marine durability, abrasion resistance, life-cycle assessment, circular construction


Abstract

Coastal protection units are subjected to combined hydraulic, mechanical, and chemical forces such as multiple wave impacts, abrasion from waves, chloride and sulfate penetration, and wetting–drying. The purpose of this study was to establish an experimental system that could be used to test alkali-activated slag (AAS) blocks using recycled seashell aggregate (RSA) as partial volumetric replacement of natural coarse aggregate (NCA). Five different mixtures were investigated: 0%, 10%, 20%, 30% and 40% seashell aggregate. The subjects included fresh state, density, compressive, splitting tensile, flexural strength, energy absorption under impact load, abrasion, and simulated marine exposure. The article included fresh state, density, compressive strength, splitting tensile strength, flexural strength, energy absorption under impact load, abrasion and simulated marine exposure. A multi-criteria framework and cradle-to-gate life cycle assessment were also identified. Since laboratory measurements are unavailable, the numerical tables of this draft explicitly include illustrative estimates (not experimental data) that underlie the proposed analysis. The illustrative scenario proposed a non-linear response, with a moderate percentage of shell incorporation as a possible compromise for both mechanical properties and waste utilization, and increased absorption for higher replacement percentages, which lead to a decrease in strength retention. These values were not experimental and were not relied upon for statistical significance or as a final optimum. The manuscript will thus be a testable experimental model and a full reporting structure, while the publication of the manuscript as an empirical article would necessitate the replacement of all simulated values with lab and life-cycle values.